In the present study, Co₃O₄ nanoparticles were synthesized by Moringa oleifera leaf extract and characterized by XRD, FTIR, SEM, EDX, and UV-Visible spectroscopy. Cobalt (II) chloride was used as the precursor with an extract-to-salt ratio of 3:1, then precipitated at a pH of 10, dried at 100 °C, and calcined at 450 °C for 3 h. XRD confirmed the formation of cubic spinel Co₃O₄ corresponding to JCPDS 42-1467 with a mean crystallite size of 21.6 ± 5.1 nm. FTIR bands at 655, 539, 472, and 418 cm⁻¹ were assigned to Co–O vibrations of the spinel structure, with other bands due to surface species from the plants. SEM revealed predominantly pseudo-cubic and polyhedral particles, with micrometer-scale aggregation and some rod-like features. EDX showed the main elements, cobalt and oxygen. UV-visible analysis showed strong absorption around 245 nm, and Tauc analysis gave a direct optical band gap of 3.31 eV. The overall results confirm the formation of crystalline Co₃O₄ with different structural, morphological, and optical properties via a Moringa oleifera-mediated route, which paves the way for further investigation in photocatalytic, sensing, and electrochemical applications.
Keywords: Co₃O₄ Nanoparticles; Moringa oleifera; Green Synthesis; Spinel Oxide; XRD; FTIR; SEM; EDX; UV–Visible Spectroscopy; Optical Band Gap